It is produced by grinding Portland clinker together with small amounts of calcium sulfate, plus a maximum of up to 35% of a combination of at least two of the following mineral additions: granulated blast furnace slag, pozzolans, and/or limestone filler. The incorporation of these additions provides the material with excellent performance in both the fresh and hardened states.
Detalle de la información
Información de la Empresa
Documento Download
EPD-IES-0028336:004 (English) EPD-IES-0028336:004 (Español)Producto que incluye esta EPD